Hubercarb® W Series Optifil® calcium carbonate has a purity level of 99.3% and is mined from a limestone deposit and processed in Quincy, IL, USA. The W Series products are ideal for applications that require high-filler loadings, low moisture content and silica content below detectable levels. In addition to being low in silica, these products are also low in trace metals like iron. Low iron content reduces undesirable degradation in some polymer systems.Information provided by Huber Engineered Materials. |