MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
RAMPF RAKU-TOOL® CP-6070 Resin / CP-6072 Hardener Epoxy paste
Categories: Polymer; Thermoset; Epoxy

Material Notes: Machine dispensed epoxy paste

Key Properties:

  • Very fine and homogeneous surface
  • Easy to machine, low dust
  • Low exotherm, can be applied over a large area in one step
  • Layer thickness 1.6 inches (40mm) without slump on vertical surfaces
Applications:
  • Molds
  • Master models
  • Design and Styling models
Cure: 7 days at RT or 14h at 104°F (40°C)

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.700 g/ccCP-6070, Resin; ASTM D-792
 0.700 g/ccCP-6072, Hardener; ASTM D-792
 0.750 g/ccCP-6070 Resin / CP-6072 Hardener; ASTM D-792
Linear Mold Shrinkage 0.0012 in/inASTM D-2566
Storage Temperature 15.0 - 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 55 - 60ASTM D-2240
Flexural Strength 13.0 - 18.0 MPaASTM D-790
Flexural Modulus 600 - 800 MPaASTM D-790
Compressive Strength 13.0 - 18.0 MPaASTM D-695
Compressive Modulus 600 - 800 MPaASTM D-695
 
Thermal PropertiesOriginal ValueComments
CTE, linear 70.0 - 75.0 µm/m-°CASTM D-3386
Deflection Temperature at 0.46 MPa (66 psi) 45.0 - 50.0 °CASTM D-648
 60.0 - 65.0 °CTest pieces were post cured at 176 F° (80°C) for 14 hours.; ASTM D-648
Glass Transition Temp, Tg 50.0 - 55.0 °C
 70.0 - 75.0 °CTest pieces were post cured at 176 F° (80°C) for 14 hours.
 
Processing PropertiesOriginal ValueComments
Pot Life 50.0 - 60.0 min4.2 lbs
 
Descriptive Properties
AspectBrown
ColorBrownCP-6070, Resin
 WhiteCP-6072, Hardener
Mix Ratio100:100CP-6070, Resin
 100:100CP-6072, Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRAMPF200 / 317800

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.