MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® 1SBVX-50H nat Nylon 1010, 50% Glass Fiber Reinforced, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Availability: Asia Pacific; Europe; North America

Filler/Reinforcement: Glass Fiber, 50% Filler by Weight

Additive: Heat Stabilizer

Features: Good Flow; Good Mold Release; Heat Stabilized; Renewable Resources Content

Uses: Appliance Components; Automotive Applications; Automotive Exterior Parts; Connectors; Consumer Applications; Electrical/Electronic Applications; Engineering Parts; Household Goods; Hydraulic Applications; Industrial Applications; Medical Devices; Pneumatic Applications; Power/Other Tools; Sporting Goods

Appearance: Natural

Forms: Granules

Processing Method: Injection Molding

Information provided by EMS-Grivory

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ISO 1183
Water Absorption 0.60 %0.60 %Equilibrium, 50% RH; ISO 62
Water Absorption at Saturation 2.0 %2.0 %ISO 62
Linear Mold Shrinkage, Flow 0.0040 cm/cm0.0040 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0010 cm/cm0.0010 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 200 MPa29000 psiISO 527-2
Elongation at Break 3.0 %3.0 %ISO 527-2
Tensile Modulus 14.5 GPa2100 ksiISO 527-1
Charpy Impact Unnotched  8.40 J/cm²
@Temperature -30.0 °C
40.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 10.1 J/cm²
@Temperature 22.8 °C
48.0 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eU
Charpy Impact, Notched  1.81 J/cm²
@Temperature -30.0 °C
8.60 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.99 J/cm²
@Temperature 22.8 °C
9.50 ft-lb/in²
@Temperature 73.0 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Comparative Tracking Index 600 V600 VIEC 60012
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 10.1 µm/m-°C5.60 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 79.2 µm/m-°C44.0 µin/in-°FISO 11359-2
Melting Point 200 °C392 °F10ºC/min; ISO 11357-3
Maximum Service Temperature, Air 100 °C212 °FLong Term; ISO 2578
 150 °C302 °FShort Term
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FUnannealed; ISO 75-2/A
Deflection Temperature at 8.0 MPa 160 °C320 °FUnannealed; ISO 75-2/C
Flammability, UL94 HB
@Thickness 0.762 mm
HB
@Thickness 0.0300 in
IEC 60695-11-10,-20

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGRIM256 / 307615

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.