MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

DuPont Mobility and Materials TPSiV® 4000-60A GFR TPV
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes:

Information provided by DuPont.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0394 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.025 cm/cm0.025 in/inISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inISO 294-4, 2577
Melt Flow 12 g/10 min12 g/10 minISO 1133
Spiral Flow 28.0 cm
@Pressure 8.00 MPa
11.0 in
@Pressure 1160 psi
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 7.00 MPa1020 psiCross direction; ISO 527-1/-2 or ISO 37
Tensile Stress at Strain  2.30 MPa
@Strain 100 %
334 psi
@Strain 100 %
Cross direction; ISO 527-1/-2 or ISO 37
 3.90 MPa
@Strain 300 %
566 psi
@Strain 300 %
Cross direction; ISO 527-1/-2 or ISO 37
Elongation at Break >= 300 %>= 300 %Cross direction; ISO 527-1/-2 or ISO 37
Tear Strength 36.0 kN/m205 plinormal; ISO 34-1
Compression Set  29 %
@Temperature 23.0 °C,
Time 86400 sec
29 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 815
 73 %
@Temperature 70.0 °C,
Time 86400 sec
73 %
@Temperature 158 °F,
Time 24.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Melt Temperature 185 °C365 °FOptimum, Injection
 185 - 205 °C365 - 401 °FRange, Extrusion
Mold Temperature 30.0 °C86.0 °FOptimum, Injection
 20.0 - 40.0 °C68.0 - 104 °FInjection
Drying Temperature 85.0 °C185 °FInjection
 85.0 °C185 °FExtrusion
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hourExtrusion, Dehumidified Dryer
 2.00 - 4.00 hour2.00 - 4.00 hourInjection, Dehumidified Dryer
 
Descriptive Properties
CompatibilityAcrylic Polymers
 Polycarbonate
 Styrenics
Drying RecommendedyesInjection
Max. screw tangential speed (m/s)0.4Injection
PolymerTPV
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDSX4902a / 291009

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.