Impact resistant polyurethane Key Properties: - Excellent physical properties
- Free of mercury, MOCA or TDI
- Phthalate free
- UL94 V-0 certified
- FAR 25.853 certified
Applications: - For room temperature hand-batch systems or vacuum-assisted casting methods
Cure 1: 1 hour at 150°F + 24 hours at 77°F Cure 2: 7 days at 77°FInformation provided by © RAMPF Tooling Solutions GmbH & Co. KG |