System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Syensqo (Solvay Specialty Polymers) Solef® 11010 PVDF
Categories:
Polymer
;
Thermoplastic
;
Fluoropolymer
;
Polyvinylidene Fluoride (PVDF)
;
Polyvinylidinefluoride (PVDF), Molded/Extruded
Material Notes:
Solef® 11010 PVDF is a medium-viscosity flexible PVDF copolymer resin and is typically processed by extrusion.
Features: Copolymer; Good Flexibility; Medium Viscosity
Information provided by Solvay Specialty Polymers.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.75
-
1.80
g/cc
ASTM D792
Water Absorption
<= 0.040 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow
0.020
-
0.030
cm/cm
ASTM D955
Melt Flow
4.0
-
8.0
g/10 min
@Load 5.00 kg,
Temperature 230 °C
ASTM D1238
Mechanical Properties
Original Value
Comments
Hardness, Shore D
70 - 75
@Thickness 2.00 mm,
Time 1.00 sec
ASTM D2240
Tensile Strength at Break
20.0
-
40.0
MPa
@Thickness 2.00 mm
50 mm/min,Type IV; ASTM D638
Tensile Strength, Yield
20.0
-
35.0
MPa
@Thickness 2.00 mm
50 mm/min,Type IV; ASTM D638
Elongation at Break
200 - 600 %
@Thickness 2.00 mm
50 mm/min,Type IV; ASTM D638
Elongation at Yield
10 - 12 %
@Thickness 2.00 mm
50 mm/min,Type IV; ASTM D638
Tensile Modulus
800
-
1200
MPa
@Thickness 2.00 mm
1.0 mm/min, Type IV; ASTM D638
Izod Impact, Notched
150
-
250
J/m
@Thickness 4.00 mm
ASTM D256
Coefficient of Friction, Dynamic
0.15 - 0.35
vs. Itself; ASTM D1894
Coefficient of Friction, Static
0.20 - 0.40
vs. Itself; ASTM D1894
Taber Abrasion, mg/1000 Cycles
5.0 - 15
CS-10 Wheel, 1000 g, 1000 Cycles; ASTM D1044
Electrical Properties
Original Value
Comments
Volume Resistivity
>=
1.00e+14
ohm-cm
ASTM D257
Surface Resistance
>=
1.00e+14
ohm
ASTM D257
Dielectric Constant
7.0 - 10
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength
20.0
-
25.0
kV/mm
@Thickness 1.00 mm
ASTM D149
Dissipation Factor
0.20
@Frequency 1e+6 Hz
ASTM D150
Thermal Properties
Original Value
Comments
Heat of Fusion
35.0
-
40.0
J/g
ASTM D3417
CTE, linear, Parallel to Flow
180
µm/m-°C
@Temperature 0.000 - 40.0 °C
ASTM D696
Specific Heat Capacity
1.20
J/g-°C
@Temperature 23.0 °C
ASTM C351
1.60
J/g-°C
@Temperature 100 °C
ASTM C351
Thermal Conductivity
0.190
W/m-K
ASTM C177
Melting Point
158
-
162
°C
Crystallization Temperature
115
-
130
°C
Peak; ASTM D3418
Vicat Softening Point
90.0
-
105
°C
Rate A (50°C/h), Loading 2 (50 N); ASTM D1525
Glass Transition Temp, Tg
-35.0
°C
ASTM E1356
Flammability, UL94
V-0
@Thickness 0.100 mm
Oxygen Index
44 %
@Thickness 3.00 mm
ASTM D2863
Descriptive Properties
Availability
Asia Pacific
Europe
Latin America
North America
Processing
Extrusion
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSOL8Y4466 / 280266
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.