MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Mocom (ALBIS) ALTECH® PC ECO 2010/121 GF10 IM UV PC, 10% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled; Polycarbonate, Impact Modified

Material Notes: Base Polymer: Polycarbonate

Filler/Additive System: 10% glass fibers, impact modified

Special Features: UV stabilized, easy release (demolding), contains recycled material

Market Segment: Automotive, various

Application Area: Exterior parts, various

Typical Applications: Housings, racking/shelving, various

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.30 g/ccISO 1183
Maximum Moisture Content 0.020
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
@Time 86400 sec
ISO 294-4
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
@Time 86400 sec
ISO 294-4
Melt Flow 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 68.0 MPaISO 527
Elongation at Break 4.5 %ISO 527
Tensile Modulus 3900 MPaISO 527
Charpy Impact Unnotched 60.0 kJ/m²ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 145 °CB50; ISO 306
 
Processing PropertiesOriginal ValueComments
Melt Temperature 310 - 330 °CInjection molding
Mold Temperature 80.0 - 130 °CInjection molding
Drying Temperature 100 - 120 °C
@Time 7200 - 10800 sec
in a dry air (desiccant) dryer
 100 - 120 °C
@Time 14400 - 43200 sec
in an circulating dryer
 
Descriptive Properties
Base PolymerPolycarbonate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eurotec® Tecotek® PC40 GR10 NL PC, 10% glass fiber reinforced, natural
Eurotec® Tecotek® PC50 GR10 GR053 FA20 PC, 10% glass fiber reinforced, flame retardant - halogen (RoHS compliant), grey RAL 9002
Eurotec® Tecotek® PC43 GR10 BK002 PC, 10% glass fiber reinforced, black
Cheng Yu Plastic ML3410 PC, 10% Glass Fiber
LATI Latiohm 87/28-05 PD01 G/10 PC, 10% Glass Fiber Reinforced

PALBIS8294 / 242353

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.