System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
SABIC LNP™ LUBRICOMP™ Compound DFL32XXP Polycarbonate (PC) (Americas)
Categories:
Polymer
;
Thermoplastic
;
Polycarbonate (PC)
Material Notes:
LNP LUBRICOMP DFL32XXP compound is based on Polycarbonate (PC) resin containing 10% glass fiber and 15% PTFE. Added features of this grade include: Wear Resistant.
Features: Wear resistant
Information provided by SABIC
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
1.37
g/cc
ASTM D792
Moisture Absorption
0.0200 %
Injection Molding
0.110 %
23°C/50% RH/24 hrs; ASTM D570
0.170 %
23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow
0.0020
cm/cm
24hrs; ASTM D955
0.0023
cm/cm
24hrs; ISO 294
Linear Mold Shrinkage, Transverse
0.0067
cm/cm
24hrs; ISO 294
0.0070
cm/cm
24hrs; ASTM D955
Mechanical Properties
Original Value
Comments
Tensile Strength at Break
71.0
MPa
ISO 527
73.0
MPa
ASTM D638
Elongation at Break
2.8 %
ISO 527
3.1 %
ASTM D638
Tensile Modulus
4100
MPa
1 mm/min; ISO 527
4350
MPa
50 mm/min; ASTM D638
Flexural Strength
114
MPa
ISO 178
123
MPa
ASTM D790
Flexural Modulus
4170
MPa
ISO 178
4350
MPa
ASTM D790
Izod Impact Notched
90.0
J
ASTM D256
Izod Impact, Unnotched
534
J/m
ASTM D4812
Izod Impact, Notched (ISO)
10.0
kJ/m²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO)
34.0
kJ/m²
80*10*4; ISO 180/1U
Dart Drop, Total Energy
11.0
J
peak; ASTM D3763
Impact Test
4.00
J
Multiaxial Impact; ISO 6603
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
140
°C
Flatw 80*10*4 sp=64mm; ISO 75/Af
141
°C
@Thickness 3.20 mm
unannealed; ASTM D648
Processing Properties
Original Value
Comments
Zone 2
310
-
320
°C
Zone 3
320
-
330
°C
Melt Temperature
305
-
325
°C
Injection Molding
Mold Temperature
80.0
-
110
°C
Drying Temperature
120
°C
Injection Molding
Dry Time
4.00
hour
Injection Molding
Back Pressure
0.200
-
0.300
MPa
Screw Speed
30
-
60
rpm
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PSABH80703 / 288650
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.