Key Features: - Convenient handling
- Versatile cure schedules
- Non halogenated filler
- UL94HB flame retardant
Master Bond has developed an epoxy system that is UL tested as per Standard 746A. When EP21AC was cured at a thickness of 3.0 mm, it withstood 150 arcs without ignition, thereby achieving an HAI PLC of 0. It also passed the UL94HB flammability test.EP21AC is a two component, room temperature curing epoxy formulated to optimize arc resistance. It is a flowable system with an easy to use 1:1 mix ratio by weight with a relatively long working life at ambient temperature. It cures at 75°F in 2-3 days or 2-3 hours 150-175°F. The optimum cure schedule is overnight at ambient temperature followed by 4-6 hours at 135-165°F. EP21AC has low shrinkage upon cure along with excellent dimensional stability. It bonds well to a wide variety of substrates, including metals, glass, ceramics and many plastics. It has exceptional durability, toughness and strength. It will resist thermal cycling and is serviceable over the temperature range of -60°C to +90°C. It has good chemical resistance to water, oils, fuels, acids and bases. Part A is translucent and the color of Part B is light yellow. In summary, EP21AC is a user friendly, two part epoxy, that meets the exceptionally demanding requirements of the arcing component of UL Standard 746A. This system can be utilized in electronic, electrical, aerospace, specialty OEM and virtually any situation where electrical arcing might be a concern. Product Advantages: - Convenient processing, 1:1 mix ratio by weight
- Good flow properties
- Flame retardant as per UL94HB
- Has a UL746A PLC rating of 0 by resisting 150 arcs without igniting
Information provided by Master Bond. |
Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.Click here to view all available suppliers for this material. Please click here if you are a supplier and would like information on how to add your listing to this material. |