MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Aquivion® PW79S-Li PFSA Lithium Salt, Coarse powder
Categories: Polymer; Thermoplastic; Fluoropolymer

Material Notes: Coarse powder, lithium sulfonate form, stabilized

Aquivion® PW79S-Li is a coarse powder based on the short-side-chain (SSC) copolymer of Tetrafluoroethylene and the Sulfonyl Fluoride Vinyl Ether (SFVE) CF2=CF-O-(CF2)2-SO2F produced by Solvay. The resulting perfluoropolymer's functional groups are in their lithium sulfonate form, SO3Li. Aquivion® PW79S-Li is chemically stabilized (denoted by the S-suffix).

This material is characterized by a low equivalent weight and a high ionic exchange capacity. It is insoluble in water, acids or bases and in most solvents unless extreme conditions would be applied.

Aquivion® PW79S-Li can be mechanically processed into blends, films or substrate coatings and preferably accompanied or followed by a heat treatment. Furthermore, It can be dissolved in organic solvents that are dipolar aprotic such as N-ethyl-2-pyrrolidone (NEP) and dimethyl sulfoxide. To facilitate the dissolution, slightly increase the temperature to 50-60°C.

For casting processes you can also consider Aquivion® D79-25BS-Li dispersion. Aquivion® powders are not harmful if used and handled according to standard processing procedures, such as those outlined in "The Guide to the Safe Handling of Fluoropolymer Resins" issued by the Society of the Plastics Industry. If handled inappropriately, powders may release harmful toxic chemicals.

PACKAGING, SHIPMENT AND STORAGE
- Aquivion® powders are delivered in standard polypropylene bottles and drums. Products should be kept closed in their original packaging.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
ColorWhite
Equivalent Weight (EW) g/eq770 to 810
FormsPowder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4142 / 279942

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.