MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Radici Radiflam® A FR 100 NT Polyamide 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced, Flame Retardant

Material Notes: PA66 flame retardant, injection molding grade. Halogen and phosphorus free. Natural color.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.17 g/ccISO 1183
Water Absorption 7.7 %
@Thickness 2.00 mm
Immersion @ 23°C; ISO 62
Moisture Absorption 1.80 %
@Thickness 2.00 mm,
Temperature 23.0 °C
50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.011 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.011 cm/cmISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 50.0 MPa50mm/min. Conditioned; ISO 527-2/1A
 77.0 MPa50mm/min. DAM; ISO 527-2/1A
Elongation at Break 12 %50 mm / min. Nominal. DAM; ISO 527-2/1A
 >= 50 %50 mm / min. Nominal. Conditioned; ISO 527-2/1A
Tensile Modulus 2600 MPa1mm / min. Conditioned; ISO 527-2/1A
 3450 MPa1mm / min. DAM; ISO 527-2/1A
Flexural Strength 115 MPa2mm / min. DAM; ISO 178
Flexural Modulus 3200 MPa2mm / min. DAM; ISO 178
Charpy Impact Unnotched 7.50 J/cm²
@Temperature 23.0 °C
DAM; ISO 179/1e/U
 12.0 J/cm²
@Temperature 23.0 °C
Conditioned; ISO 179/1e/U
Charpy Impact, Notched 4.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1e/A
 4.50 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1e/A
 6.50 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1e/A
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned. 500V; IEC 60093
 1.00e+13 ohm-cmDAM; 500V.; IEC 60093
Surface Resistance 1.00e+10 ohmConditioned. 500V; IEC 60093
 1.00e+12 ohmDAM; 500V.; IEC 60093
Dielectric Strength 26.0 kV/mmConditioned; IEC 60243-1
 31.0 kV/mmDAM; IEC 60243-1
Comparative Tracking Index 600 VDAM. Sol.A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 200 °CISO 75/2Bf
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °CISO 75/2Af
Vicat Softening Point 220 °C
@Load 5.10 kg
50°C/h; ISO 306
Flammability, UL94 V-0
@Thickness 0.800 mm
 V-0
@Thickness 0.400 mm
Flame Spread 0.000 mm/min
@Thickness 3.00 mm
Automotive Interior; ISO 3795
Smoke Density 35
@Thickness 1.00 mm
Ds max. 25kW/m2 w/ pilot flame; EN ISO 5659-2
Oxygen Index 35 %ISO 4589-2
Glow Wire Ignition Temperature >= 750 °C
@Thickness 2.00 mm
IEC 60695-2-1/3
 >= 775 °C
@Thickness 1.00 mm
IEC 60695-2-1/3
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC 60695-2-1/2
 960 °C
@Thickness 2.00 mm
IEC 60695-2-1/2
 
Processing PropertiesOriginal ValueComments
Processing Temperature 270 - 290 °CExtrusion Temperature
Melt Temperature 270 - 290 °CInjection Molding
Mold Temperature 60.0 - 80.0 °C
Aging Temperature 121 °C
@Time 7.20e+7 sec
TI @ 50% loss of Tensile Strength; ISO 2578
 134 °C
@Time 7.20e+7 sec
TI @ 50% loss of Tensile Strength; ISO 2578
 151 °C
@Time 1.80e+7 sec
TI @ 50% loss of Tensile Strength; ISO 2578
 186 °C
@Time 1.80e+7 sec
TI @ 50% loss of Dielectric Strength; ISO 2578
 
Descriptive Properties
CITnlp Conv. Index of Toxicity0.45NF X70-100-1/2. Not listed product (600°C)
EN 45545-2 ClassificationR23 HL3EN 45545-2. 1mm.
Injection Molding Injection SpeedMedium
NF ClassificationI2/F2NF F16-101

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRADI6981 / 293486

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.