MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Alfa Chemistry Materials Bismuth single crystal, 15mm (0.59in) dia, 25mm (1in) long, (100) orientation
Categories: Metal; Nonferrous Metal; Bismuth Alloy

Material Notes:

Information provided by Alfa Chemistry Materials.

Vendors: Alfa Chemistry is an ISO 9001:2015 certified supplier of various materials, including: MOFs, coatings, nanomaterials, metals, polymers, carbon fibers, graphite, ceramics, glass, semiconductors, catalysts, carbon nanotubes, fullerene, COFs, molecular sieve, quantum dots, recycled plastics, photonic and optical materials, and magnetic materials, for customers worldwide. Alfa Chemistry also provides custom synthesis services for nearly all kinds of materials and chemicals. Learn more about Alfa Chemistry's high quality products at materials.alfachemic.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 9.747 g/cc0.3521 lb/in³
Molecular Weight 208.98 g/mol208.98 g/mol
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 32.0 GPa4640 ksi
Poissons Ratio 0.330.33
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.000129 ohm-cm
@Temperature 20.0 °C
0.000129 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 54.1 J/g23.3 BTU/lb
Heat of Vaporization 723 J/g311 BTU/lb
CTE, linear 13.4 µm/m-°C
@Temperature 25.0 °C
7.44 µin/in-°F
@Temperature 77.0 °F
Specific Heat Capacity 0.123 J/g-°C
@Temperature 20.0 °C
0.0294 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 7.97 W/m-K55.3 BTU-in/hr-ft²-°F
Melting Point 271.3 °C520.3 °F
Boiling Point 1560 °C2840 °F
 
Descriptive Properties
Alfa Chemistry Materials CategoryMetals and Materials
AppearancePowder
CAS Number7440-69-9
EC Number231-177-4
Electronegativity2.02 Paulings
GHS Precautionary StatementsP210-P370 + P378
GHS Safety Description16
Hazard CodesH228
MDL NumberMFCD00134033
Molecular FormulaBi
Purity99%, 99.9%, 99.99%, 99.999%
Risk Codes11
Signal WordWarning
UN NumberUN 3089 4.1/PG 2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

ZZALFA0821 / 269876

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.