MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ ELCRES™ CRX9411W Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP ELCRES CRX9411W is an amorphous PC copolymer resin that offers medium flow, UL V0 rating @ 1.6 mm for all colors, and high ductility in combination with excellent chemical resistance. CRX9411W is available for custom coloring and may be an excellent candidate for a wide variety of applications that need improved chemical resistance. This grade is subjected to SABIC healthcare management of change policy and formulation lock.

Features: Healthcare,Enhanced Ductility,Enhanced Chemical Resistance,Flame Retardant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
Viscosity 9.5 cP
@Load 1.20 kg,
Temperature 300 °C
MVR cc/10 min; ASTM D1238
Linear Mold Shrinkage, Flow 0.0040 - 0.0090 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0090 cm/cmSABIC method
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 52.0 MPa50 mm/min; ASTM D638
Elongation at Break >= 100 %50 mm/min; ASTM D638
Elongation at Yield 6.0 %50 mm/min; ASTM D638
Tensile Modulus 1920 MPa50 mm/min; ASTM D638
Flexural Strength 85.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2000 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 765 JASTM D256
 570 J
@Temperature -70.0 °C
ASTM D256
 609 J
@Temperature -60.0 °C
ASTM D256
 680 J
@Temperature -30.0 °C
ASTM D256
Dart Drop, Total Energy 61.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 175 - 250 VUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 125 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 142 °CRate B/50; ASTM D1525
 146 °CRate B/120; ASTM D1525
Flammability, UL94 V-0
@Thickness >=1.60 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 290 - 340 °C
Zone 2 280 - 330 °C
Zone 3 290 - 340 °C
Melt Temperature 290 - 340 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 12.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 80 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 50 - 100 rpm
 
Descriptive Properties
Instrumented Dart Impact Ductility, 23°C100 %ASTM D3763

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH80588 / 288535

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.