MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Daikin DAI-EL® T-530 Thermoplastic Fluoroelastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Fluoropolymer

Material Notes: DAI-EL® T-530 is a thermoplastic elastomer that has rubber-like elasticity yet processes like a thermoplastic. DAI-EL® T-530 is transparent and low in extractables. It is USP Class VI certified. DAI-EL® T-530 exhibits excellent physical properties and chemical resistance without crosslinking, but where sealing ability is required it may be crosslinked by e-beam radiation.

Typical Applications: Tubing, sheets, o-rings and other parts for chemical, food and pharmaceuticals contact

Features: Good transparency, excellent chemical resistance

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.89 g/cc
Melt Flow 22 g/10 min
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 67
Tensile Strength at Break 10.8 MPa
Elongation at Break 650 %
100% Modulus 1.90 MPa
@Strain 100 %
Compression Set 23 %
@Temperature 150 °C,
Time 252000 sec
150 KGy Radiation
 34 %
@Temperature 150 °C,
Time 252000 sec
100 KGy Radiation
 57 %
@Temperature 150 °C,
Time 252000 sec
30 KGy Radiation
 65 %
@Temperature 150 °C,
Time 252000 sec
10 KGy Radiation
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 5.00e+13 ohm-cm
Dielectric Constant 6.6
@Frequency 1000 Hz
Dielectric Strength 14.0 kV/mm
 
Thermal PropertiesOriginal ValueComments
Specific Heat Capacity 1.23 J/g-°C
Thermal Conductivity 0.000360 cal cm/sec-cm²-°C
Melting Point 230 °C
Minimum Service Temperature, Air -9.00 °CGehman Torsion T50
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Descriptive Properties
AppearanceTranslucent Pellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Advanced Elastomer Systems Santoprene® 181-55 Thermoplastic Rubber
AGC AFLAS® 150L TFE/P Fluoroelastomers
Avient Trilliant™ HC HC0200-5001 XR Grey Thermoplastic Elastomer (TPE)
3M Dyneon™ PFE 300Z Clear Perfluoroelastomer System
Advanced Elastomer Systems Santoprene® 281-64 Thermoplastic Rubber

PDAIJ9873 / 209944

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.