MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ITW Chockfast® PHILLYCLAD 5066A Epoxy Coating
Categories: Polymer; Thermoset; Epoxy

Material Notes: Phillyclad 5066A is a two component, heavy duty coating designed for applications requiring a high degree of resiliency combined with excellent adhesion and impact properties. The compound is resistant to oils, fuels and most chemicals, is nontoxic and contains no volatiles. Phillyclad 5066A is self extinguishing and meets the requirements of ASTM D635. Typical applications include the coating of lagging or insulation on piping, boilers, valves, etc. to prevent the absorption of oils and the associated fire hazard. Phillyclad 5066A is designed to protect monolithic types of insulation and other semiresilient substrates from abuse or damage. Easily applied at thicknesses up to 6mm, this product seals out contaminants while providing a tough resilient coating highly resistant to heat, impact or other damage.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Cure Time <= 4.00 houron hot surface
Pot Life 240 min
@Temperature 21.1 °C
 
Descriptive Properties
Colorblackhardener
 dark graymixed
 whiteresin
ViscosityMastic Paste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWC9038 / 239548

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.