Lord 200 Series Lord 200 Series Acrylic Adhesives bond minimally prepared or unprepared surfaces. They offer excellent adhesion to unprepared metals, ceramic magnets and plastics. Viscosities range from paste to liquid. Cure times range from 2 to 35 minutes.
Lord Adhesives 206 Long Working Time Acrylic Adhesive |