MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Ex-Tech Plastics VersaTech™ APET
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET)

Material Notes: Ex-Tech VersaTech™ APET has exceptional properties such as visual transparency high heat distortion and it has good resistance to mineral oils, solvents and acids.

Characteristics:
Transparent
Exceptional visual properties
Superior performance in critical consumer applications

End Uses:
Food and medical trays
Consumer packaging: clamshell, blister and tray

Information provided by Ex-Tech Plastics Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.33 g/cc
Viscosity Measurement >= 0.75Intrinsic Viscosity; ASTM D3835
Linear Mold Shrinkage 0.020 - 0.050 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 58.6 MPaASTM D638
Elongation at Break 250 %
Flexural Modulus 350000 psiASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point >= 240 °C
 
Optical PropertiesOriginal ValueComments
Haze <= 2.0 %ASTM D1003
Transmission, Visible >= 90 %ASTM D1003
 
Descriptive Properties
Clarity>99%ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ex-Tech Plastics VersaTech™ RPET Packaging Polymer
Spartech APET SP4110 Copolyester Sheet
Celanese Rynite® 408 NC010 PET
Envalior Arnite® A02 307 PET
Celanese Rynite® 408 NC010 PET (Extended Tabular Temperature Data)

PEXTEC992 / 133217

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.