Compound 23718 is a 70 durometer black colored EPDM elastomer, it is formulated with Teflon to provide internal lubrication. It exhibits good resistance to heat , compression set and boiling water. It will remain non brittle at low temperatures. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 AA 715 A13 EA14 F17; 3 AA 715 B13 B33 EA14 F17 G21; 4 AA 715 A13 B13 B33 EA14 F17 G21 F17; 5 AA 715 A13 B13 B33 EA14 F17 G21; 2 BA 715 F17; 3 BA 715 A14 B13 F17 F19; 4 BA 715 A14 F17; 5 BA 715F17 F19; 4 CA 715 A25 B35 EA14 F17 F18 F19 G21; 5 CA 715 A25 B35 EA14 F17 F18 G11 G21Information provided by Pressure Seals Inc. |