Z-PEI 9085 is a durable, aerospace-grade polymer with strength-to-weight ratio comparable to aluminum 6061. This filament consists of polyetherimide with a polycarbonate copolymer blend. Z-PEI 9085 exhibits excellent thermal properties and retains its properties in temperatures reaching 170° C . The most notable property of Z-PEI 9085 is very low FST (Flame, Smoke, Toxicity). The material has a UL 94 V-0 flammability rating which makes it perfect for printing flame-retardant components. Applications: - industrial parts and tools
- aerospace interiors
- ductwork
- flame-retardant components
Information provided by Zortrax |