MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chengdu Letain LTP ZC-1600B PPS, High toughness
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: LTP T serials coatings of LETIAN Plastics have excellent resistance to abrasion and corrosion, its adhesive power reach grade 0, impact strength is above 5MPa, hardness reach to HRA80, salt spray test exceed 300 hours, application at moderate temperature, easy to construction, bright appearance.

Information provided by Chengdu Letain Plastic

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 165 MPa23900 psi
Elongation at Break 1.6 %1.6 %
Flexural Strength 220 MPa31900 psi
Flexural Modulus 14.2 GPa2060 ksi
Izod Impact, Notched (ISO) 9.00 kJ/m²4.28 ft-lb/in²
Izod Impact, Unnotched (ISO) 45.0 kJ/m²21.4 ft-lb/in²
 
Descriptive Properties
Melt index25-60 g
Resistance to heat leap200

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHENGLT004 / 255857

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.