MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Ascend Performance Materials Vydyne® 49H BK0743 PA66-I
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Impact Grade

Material Notes: Vydyne 49H BK0743 is a general-purpose, impact-modified, high modulus PA66 resin. 49H BK0743 is recognized for all the processing and property advantages inherent to PA66 with the addition of improved impact strength. This resin offers a well balanced combination of engineering properties characterized by high melt point, good surface lubricity, abrasion resistance, resistant to most chemicals including motor oils, transmission fluids, lubricants and fuels.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³DAM; ISO 1183
Linear Mold Shrinkage, Flow 0.026 cm/cm
@Thickness 2.00 mm
0.026 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.022 cm/cm
@Thickness 2.00 mm
0.022 in/in
@Thickness 0.0787 in
DAM; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 45.0 MPa6530 psi50% RH; ISO 527-2
 71.0 MPa10300 psiDAM; ISO 527-2
Elongation at Break 21 %21 %DAM; ISO 527-2
 84 %84 %50% RH; ISO 527-2
Tensile Modulus 1.30 GPa189 ksi50% RH; ISO 527-2
 2.70 GPa392 ksiDAM; ISO 527-2
Flexural Strength 29.0 MPa4210 psi50% RH; ISO 178
 78.0 MPa11300 psiDAM; ISO 178
Flexural Modulus 1.10 GPa160 ksi50% RH; ISO 178
 2.60 GPa377 ksiDAM; ISO 178
Izod Impact, Notched (ISO)  7.70 kJ/m²
@Temperature -40.0 °C
3.66 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 8.00 kJ/m²
@Temperature 23.0 °C
3.81 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
 8.40 kJ/m²
@Temperature -30.0 °C
4.00 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 12.0 kJ/m²
@Temperature -40.0 °C
5.71 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 180/1A
 13.0 kJ/m²
@Temperature -30.0 °C
6.19 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 180/1A
 22.0 kJ/m²
@Temperature 23.0 °C
10.5 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 180/1A
Charpy Impact Unnotched  NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -40.0 °C
NB
@Temperature -40.0 °F
DAM; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
50% RH; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
DAM; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50% RH; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.730 J/cm²
@Temperature -40.0 °C
3.47 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 179/1eA
 0.790 J/cm²
@Temperature -30.0 °C
3.76 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.910 J/cm²
@Temperature 23.0 °C
4.33 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 1.10 J/cm²
@Temperature -40.0 °C
5.23 ft-lb/in²
@Temperature -40.0 °F
50% RH; ISO 179/1eA
 1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
50% RH; ISO 179/1eA
 2.10 J/cm²
@Temperature 23.0 °C
9.99 ft-lb/in²
@Temperature 73.4 °F
50% RH; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength  31.0 kV/mm
@Thickness 1.00 mm
787 kV/in
@Thickness 0.0394 in
50% RH; IEC 60243
 31.0 kV/mm
@Thickness 1.00 mm
787 kV/in
@Thickness 0.0394 in
DAM; IEC 60243
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 197 °C387 °FUnannealed; DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 67.0 °C153 °FUnannealed; DAM; ISO 75-2/A
 87.0 °C189 °FUnannealed; 50% RH; ISO 75-2/A
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Middle Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Front Barrel Temperature 280 - 310 °C536 - 590 °FInjection
Nozzle Temperature 280 - 310 °C536 - 590 °FInjection
Melt Temperature 285 - 305 °C545 - 581 °FInjection
Mold Temperature 65.0 - 95.0 °C149 - 203 °FInjection
Drying Temperature 80.0 °C176 °FInjection
Dry Time 4.00 hour4.00 hourInjection
 
Descriptive Properties
AdditiveHeat Stabilizer
AppearanceBlack
FeaturesAbrasion Resistance
 Chemical Resistant
 Fast Molding Cycle
 Gasoline Resistant
 General Purpose
 Good Processability
 Good Toughness
 Heat Stabilized
 High Impact Resistance
 Impact Modified
 Oil Resistant
 Solvent Resistant
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe, Asia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE9230 / 287591

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.