MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Gougeon Brothers Entropy Resins® ONS High Biobased Epoxy Resin
Categories: Polymer; Renewable/Recycled Polymer; Thermoset; Epoxy

Material Notes: High Biobased Epoxy Resin for general laminations and coatings.

Product Overview: ONE is a general purpose laminating resin with high biobased content for composite laminating, coating, and adhesive applications. This system features a faster speed, low viscosity and includes quick air-releasing properties ideal for fiber-reinforced composite laminations and coatings. ONE is a USDA Certified BioPreferred® Product with 30% biobased content.

Information provided by Gougeon Brothers, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.980 g/cc0.0354 lb/in³hardener
 1.08 g/cc0.0390 lb/in³mixed
 1.14 g/cc0.0412 lb/in³resin
Volatile Organic Compounds (VOC) Content 7.7 g/l7.7 g/lASTM D2369
Viscosity 140 cP140 cPB
 1060 cP1060 cPMixed
 1870 cP1870 cPA
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 70 - 8070 - 80
Tensile Strength 67.6 MPa9800 psiASTM D638
Elongation at Break 6.0 %6.0 %ASTM D638
Tensile Modulus 3.23 GPa468 ksiASTM D638
Flexural Strength 100.5 MPa14580 psiASTM D790
Flexural Modulus 2.96 GPa430 ksiASTM D790
Compressive Strength 86.32 MPa12520 psiASTM D695
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 53.3 °C128 °FDSC, midpoint
 
Processing PropertiesMetricEnglishComments
Cure Time  480 min
@Temperature 35.0 °C
8.00 hour
@Temperature 95.0 °F
Tack Free Time
 10100 min
@Temperature 25.0 °C
168 hour
@Temperature 77.0 °F
Recommended Full Cure
Pot Life 43.0 min43.0 min
 
Descriptive Properties
Mix ratio100:43Weight
 2:1Volume
Mixed Biobased Carbon Content (%)21ASTM D6866

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOUGE983 / 290826

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.