Compound 3544 is a 50 durometer black colored Buna N elastomer, it is formulated with FDA sanctioned materials and is non-crazing on plastics. It exhibits good resistance to heat, compression set and petroleum based oils. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 BG 515 B14 B34 EA14 EF11 F17; 3 BG 515 B14; 4 BG 515 B14 EO34; 5 BG 515 A14 B14 B34 EO34 CFR21 177.2600 Information provided by Pressure Seals Inc. |