Appearance: Silver Product Benefits: - Low stress
- Improved JEDEC performance
- Fast cure
- Excellent adhesion to copper
Cure: Heat cureApplication: Die attach LOCTITE ABLESTIK 3230 electrically conductive die attach adhesive is designed for high reliability package applications . It can be used in a variety of package sizes. Information provided by Loctite® |