MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Nouryon DEZn SSG Diethylzinc
Categories: Other Engineering Material

Material Notes: DEZn SSG is a zinc precursor (Select Semiconductor Grade) for the deposition of compound semiconductors.

CAS number: 557-20-0

EINECS/ELINCS No.: 209-161-3

Applications: We offer the highest purity diethylzinc precursor under the product name of DEZn SSG (Select Semiconductor Grade). DEZn SSG is a zinc precursor for the deposition of compound semiconductors. Compound semiconductors are used in applications such as light emitting diodes and high efficiency solar cells. Containers are fabricated from stainless steel with an electropolished internal finish and are equipped with dip tube for top discharge and diaphragm valves. The diaphragm valves are equipped with metal gasket face seal connections.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.198 g/cc
Viscosity 0.70 cP
@Temperature 21.0 °C
Molecular Weight 123.5 g/mol
Vapor Pressure 0.00905 bar
@Temperature 10.0 °C
283.15 K
 0.0160 bar
@Temperature 20.0 °C
293.15 K
 
Thermal PropertiesOriginal ValueComments
Heat of Vaporization 326 J/g
@Temperature 118 °C
Specific Heat Capacity 1.502 J/g-°C
@Temperature 57.0 °C
Melting Point -30.0 °C
Boiling Point 117.6 °C
Heat of Formation 17.0 kJ/mol?Hf°, 25 °C / 1 bar
 
Descriptive Properties
AppearanceColorless liquid
Heat of combustion-3364 kJ/moleΔHc°, 25 °C
Heat of hydrolysis2117 J/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY476 / 285999

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.