MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BASF Ultraform® N 2640 Z4 BK140 Q600 POM
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: Ultraform N2640 Z4 BK140 Q600 is a high toughness, elastomer-modified injection molding POM grade.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.35 g/ccISO 1183
Water Absorption 0.80 %ISO 62
Moisture Absorption at Equilibrium 0.25 %23°C/50% R.H.; ISO 62
Linear Mold Shrinkage 0.019 cm/cmASTM Data; MD
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 36.0 MPa50mm/min; ISO 527
Elongation at Break >= 50 %50mm/min, Nominal strain; ISO 527
Elongation at Yield 14 %50mm/min; ISO 527
Tensile Modulus 1550 MPa1mm/min; ISO 527
Flexural Modulus 1570 MPaASTM Test
 1740 MPaISO Data
Izod Impact, Notched 0.950 J/cm
@Thickness 3.17 mm
ASTM Test
Izod Impact, Notched (ISO) 11.7 kJ/m²ISO Test
 
Thermal PropertiesOriginal ValueComments
Melting Point 167 °C10 K/min
 167 °CASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °CASTM Test
 
Descriptive Properties
ColorBK140
Commercial StatusActive America
Impact ModifiedYes
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultraform® N 2640 Z4 UNC Q600 POM
BASF Ultraform® N2640 E4 POM
A. Schulman CPP30GF33BK 30% Mineral Filled, Heat-Stabilized, Homopolymer Polypropylene
BASF Ultraform® N 2320 003 UNC Q600 POM
BASF Ultraform® N2320 006 POM

PBASF9107 / 84871

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.