MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Radici Radilon® A RV500RW 339 BK Polyamide 66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: PA66 50% glass fiber filled, injection molding grade. Heat stabilized. Black color. Suitable for technical parts requiring very high stiffness and high mechanical resistance. Excellent heat aging properties retention, improved welding lines strength. Especially fit for demanding metal replacement applications.

Information provided by Radici Group.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.58 g/cc0.0571 lb/in³DAM; ISO 1183
Water Absorption 4.0 %
@Thickness 2.00 mm,
Temperature 23.0 °C
4.0 %
@Thickness 0.0787 in,
Temperature 73.4 °F
Immersion; ISO 62
Moisture Absorption 1.10 %
@Thickness 2.00 mm,
Temperature 23.0 °C
1.10 %
@Thickness 0.0787 in,
Temperature 73.4 °F
50% RH; ISO 62
Viscosity Test 152 cm³/g1.52 dl/gViscosity Index; Sulfuric Acid; ISO 307
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0070 cm/cm0.0070 in/inISO 294-4
Melt Flow 8.2 g/10 min
@Load 5.00 kg,
Temperature 275 °C
8.2 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 190 MPa27600 psi5mm / min. Conditioned; ISO 527-2/1A
 240 MPa34800 psi5mm / min. DAM; ISO 527-2/1A
Elongation at Break 3.0 %3.0 %5 mm / min. DAM; ISO 527-2/1A
 3.1 %3.1 %5 mm / min. Conditioned; ISO 527-2/1A
Tensile Modulus 14.25 GPa2067 ksi1mm / min. Conditioned; ISO 527-2/1A
 17.0 GPa2470 ksi1mm / min. DAM; ISO 527-2/1A
Flexural Strength 305 MPa44200 psi2mm / min. Conditioned; ISO 178
 370 MPa53700 psi2mm / min. DAM; ISO 178
Flexural Modulus 15.4 GPa2230 ksi2mm / min. Conditioned; ISO 178
 15.5 GPa2250 ksi2mm / min. DAM; ISO 178
Charpy Impact Unnotched  10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
 10.2 J/cm²
@Temperature -30.0 °C
48.5 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 11.2 J/cm²
@Temperature 23.0 °C
53.3 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
Charpy Impact, Notched  1.70 J/cm²
@Temperature -30.0 °C
8.09 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1e/A
 2.00 J/cm²
@Temperature 23.0 °C
9.52 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1e/A
 2.50 J/cm²
@Temperature 23.0 °C
11.9 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1e/A
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cm500V, Conditioned; IEC 60093
 1.00e+13 ohm-cm1.00e+13 ohm-cm500V, DAM; IEC 60093
Surface Resistance 1.00e+10 ohm1.00e+10 ohm500V, Conditioned; IEC 60093
 1.00e+12 ohm1.00e+12 ohm500V, DAM; IEC 60093
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
8.33 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 85.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
47.2 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Thermal Conductivity 0.370 W/m-K2.57 BTU-in/hr-ft²-°FIn plane
Melting Point 260 °C500 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 255 °C491 °FISO 75/2Af
Deflection Temperature at 8.0 MPa 215 °C419 °FISO 75/2Af
Vicat Softening Point 255 °C
@Load 5.10 kg
491 °F
@Load 11.2 lb
50°C/h; ISO 306
Glow Wire Ignition Temperature  725 °C
@Thickness 1.00 mm
1340 °F
@Thickness 0.0394 in
IEC 60695-2-1/3
 725 °C
@Thickness 2.00 mm
1340 °F
@Thickness 0.0787 in
IEC 60695-2-1/3
Glow Wire Flammability Index  700 °C
@Thickness 1.00 mm
1290 °F
@Thickness 0.0394 in
IEC 60695-2-1/2
 700 °C
@Thickness 2.00 mm
1290 °F
@Thickness 0.0787 in
IEC 60695-2-1/2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 - 310 °C536 - 590 °FInjection Molding
Mold Temperature 80.0 - 100 °C176 - 212 °F
 
Descriptive Properties
Injection Molding Injection SpeedHigh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRADI6930 / 293435

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.