MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Lavanta® 5115 WH 224 High Performance (HPP), 15% glass fiber
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: 15% glass fiber, high reflectivity, SMT compatible, HB LED packaging

Lavanta® 5115 WH 224 is a 15% glass fiber reinforced, high-performance polyester (HPP) injection molding grade developed specifically for HB LED packaging applications that utilize surface mount technology.

Lavanta® 5115 WH 224 has high reflectivity with excellent whiteness retention even after thermal and light aging. This gives it excellent reliability for LEDs that operate at high junction temperatures.

- White: 5115 WH 224

Applications: LEDs

Features: Chemical Resistant; Fast Molding Cycle; Good Color Stability; High Reflectivity; High Stiffness; Light Stabilized; Low Moisture Absorption

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.62 g/ccASTM D792
Water Absorption 0.048 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0039 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.012 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Stress 73.3 MPaISO 527-2
Elongation at Break 1.5 %ISO 527-2
Tensile Modulus 6730 MPaISO 527-2
Flexural Strength 108 MPaISO 178
Flexural Modulus 6230 MPaISO 178
Izod Impact, Notched (ISO) 2.40 kJ/m²Type 1, Notch A; ISO 180
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 17.0 µm/m-°C
@Temperature 150 - 200 °C
ASTM E831
 20.0 µm/m-°C
@Temperature 200 - 250 °C
ASTM E831
 29.0 µm/m-°C
@Temperature 50.0 - 100 °C
ASTM E831
CTE, linear, Transverse to Flow 58.0 µm/m-°C
@Temperature 50.0 - 100 °C
ASTM E831
 100 µm/m-°C
@Temperature 100 - 150 °C
ASTM E831
 120 µm/m-°C
@Temperature 150 - 200 °C
ASTM E831
 140 µm/m-°C
@Temperature 200 - 250 °C
ASTM E831
Melting Point 289 °CISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 269 °CUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 214 °CUnannealed; ISO 75-2/A
 
Optical PropertiesOriginal ValueComments
Reflection Coefficient, Visible (0-1) >= 0.95ASTM E1331
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 305 °C
Front Barrel Temperature 290 °C
Melt Temperature 295 - 310 °CInjection
Mold Temperature 130 - 150 °C
Drying Temperature 120 °C
@Time 14400 sec
Moisture Content <= 0.030 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorWhite
FormsPellets
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4356 / 280156

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.