MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® HTplus M5000 natural colored Polyphthalamide (PPA)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA)

Material Notes: VESTAMID® HTplus M5000 natural colored is a neat resin for polyphthalamide (PPA) based compounds for injection molding. This base resin is especially suitable for manufacturing parts subjected to high temperature. VESTAMID® HTplus M5000 natural colored is supplied as cylindrical pellets in polyethylene packaging. Drying at 100°C for at least 4 hours before processing is recommended. Pigmentation may affect values.

Property data for dry samples unless otherwise noted.

Information provided by Evonik.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0040 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0050 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPaConditioned; ISO 527
 90.0 MPaISO 527
Tensile Strength, Yield 80.0 MPaConditioned; ISO 527
 90.0 MPaISO 527
Elongation at Break 40 %ISO 527
 120 %Conditioned. Nominal; ISO 527
 120 %Nominal; ISO 527
Elongation at Yield 5.0 %Conditioned; ISO 527
 6.0 %ISO 527
Tensile Modulus 2700 MPaISO 527
 2900 MPaConditioned; ISO 527
Charpy Impact Unnotched 180 kJ/m²
@Temperature -40.0 °C
Complete Break, Conditioned; ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eA
 9.50 kJ/m²
@Temperature 23.0 °C
Complete Break; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 28.0 kV/mmAC, S20/P50; Sim. to IEC 60243-1
Comparative Tracking Index 550 Vtest solution A, 50 drops value; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 64.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2.
CTE, linear, Transverse to Flow 61.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
Melting Point 280 °CISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 120 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 110 °CISO 75-1/-2
Glass Transition Temp, Tg 130 °CISO 11357-1/-2
Flammability Test 3.0
@Thickness 3.20 mm
IEC 60695-11-10
 3.0
@Thickness 1.60 mm
IEC 60695-11-10
 3.0
@Thickness 0.800 mm
IEC 60695-11-10
 
Processing PropertiesOriginal ValueComments
Mold Temperature 80.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEVONIK840 / 243049

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.