MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Dow ELITE™ 5960G HDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Product Description: Main Characteristics:
  • HDPE with excellent moisture barrier
  • Processes with low back pressure and excellent bubble stability

Availability: Asia Pacific; Latin America; North America

Additive: Antiblock: 3000 ppm; Processing Aid: No; Slip: No

Agency Ratings: FDA 21 CFR 177.1520©2.2; HPFB (Canada) No Objection; EU No 10/2011

Form: Pellets

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.964 g/ccASTM D792
Melt Flow 0.85 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 3000 ppm
 
Mechanical PropertiesOriginal ValueComments
Puncture Resistance 3.00 lb (f)
Film Tensile Strength at Yield, MD 4100 psiASTM D882
Film Tensile Strength at Yield, TD 4400 psiASTM D882
Film Elongation at Break, MD 500 %ASTM D882
Film Elongation at Break, TD 600 %ASTM D882
1% Secant Modulus 163000 psiMD; ASTM D882
 193000 psiTD; ASTM D882
2% Secant Modulus 127000 psiMD; ASTM D882
 148000 psiTD; ASTM D882
Puncture Energy 3.00 in-lb
Elmendorf Tear Strength MD 13 gASTM D1922
Elmendorf Tear Strength TD 400 gASTM D1922
Dart Drop Test 40.0 gASTM D1709A
Film Tensile Strength at Break, MD 5400 psiASTM D882
Film Tensile Strength at Break, TD 3500 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 273 °F
Vicat Softening Point 266 °FASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 42 %ASTM D1003
Gloss 14 %45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 425 °FExtrusion
Blow-up Ratio (BUR) 2.5
 
Descriptive Properties
Film Puncture Resistance17 ft-lb/in3
Film Toughness1550 ft-lb/in3TD, ASTM D882
 1700 ft-lb/in3MD, ASTM D882

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF502 / 311195

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.