MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ITW Spraycore® SC 7315 Coring / Bulk Print Blocker
Categories: Polymer; Thermoset

Material Notes: SC 7315 is a unique micro balloon syntactic resin that can be used in a variety of ways to enhance the cosmetic appearance, rigidity, and speed of production of fiberglass reinforced plastic products. It is an attractive alternative to other core materials such as plywood, PVC, foams, end grained balsa and polyester mats. SC 7315 is sprayed into place at the desired thickness and is typically lower in cost that other core materials. MEKP catalyst is not included. Product features: reduces fiberglass print, formulated for adjustable densities, excellent hang on vertical surfaces, high build material. Product benefits: speeds up production, lowers finishing costs, economical alternative to more expensive coring materials. Preferred red dye catalyst: HP 90, HP 90

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.80 - 6.30 lb/galApplication density
Viscosity 10000 - 14000 cPRVF #5 @ 20rpm
 
Chemical PropertiesOriginal ValueComments
Styrene Content 32 %
 
Processing PropertiesOriginal ValueComments
Gel Time 0.500 - 1.50 minwith HP-90 Catalyst and 2.0% MEKP/1.50% MR-100 Mix Ratio
 4.00 - 8.00 minwith HP-90 Catalyst and 1.50% MEKP Mix Ratio
 4.00 - 8.00 minGel to Peak with HP-90 Catalyst and 2.0% MEKP/1.50% MR-100 Mix Ratio
 6.00 - 10.0 minGel to Peak with HP-90 Catalyst and 1.50% MEKP Mix Ratio
 
Descriptive Properties
ColorOff white
Peak Exotherm300 to 350°F100g mass

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWS9064 / 239574

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.