MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ascend Performance Materials Vydyne® A28 PA66
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Vydyne A28 is an unreinforced, PA66 for injection molded applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³DAM; ISO 1183
Moisture Absorption at Equilibrium 2.0 %2.0 %DAM to 50% RH; ISO 62
Water Absorption at Saturation 8.5 %8.5 %ISO 62
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 20.0 MPa2900 psiDAM; ISO 527-2
Tensile Strength, Yield 85.0 MPa12300 psiDAM; ISO 527-2
Elongation at Yield 3.8 %3.8 %DAM; ISO 527-2
Tensile Modulus 3.00 GPa435 ksiDAM; ISO 527-2
Flexural Strength 105 MPa15200 psiDAM; ISO 178
Flexural Modulus 2.80 GPa406 ksiDAM; ISO 178
Izod Impact, Notched (ISO)  3.00 kJ/m²
@Temperature -40.0 °C
1.43 ft-lb/in²
@Temperature -40.0 °F
DAM; ISO 180/1A
 3.00 kJ/m²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 180/1A
 5.00 kJ/m²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 180/1A
Charpy Impact Unnotched  10.0 J/cm²
@Temperature -30.0 °C
47.6 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eU
 27.0 J/cm²
@Temperature 23.0 °C
128 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
DAM; ISO 179/1eA
 0.500 J/cm²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
DAM; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm
@Thickness 1.00 mm
1.00e+16 ohm-cm
@Thickness 0.0394 in
DAM; IEC 60093
Comparative Tracking Index 600 V
@Thickness 3.00 mm
600 V
@Thickness 0.118 in
IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 35.0 - 55.0 °C
44.4 µin/in-°F
@Thickness 0.0787 in,
Temperature 95.0 - 131 °F
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
44.4 µin/in-°F
@Thickness 0.0787 in,
Temperature 73.4 - 131 °F
DAM; ISO 11359-2
Oxygen Index 26 %26 %DAM; EN ISO 4589-2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 260 - 270 °C500 - 518 °FInjection
Middle Barrel Temperature 270 - 280 °C518 - 536 °FInjection
Front Barrel Temperature 270 - 290 °C518 - 554 °FInjection
Melt Temperature 270 - 290 °C518 - 554 °FInjection
Mold Temperature 60.0 - 90.0 °C140 - 194 °FInjection
Drying Temperature 75.0 - 85.0 °C167 - 185 °FInjection
Dry Time 4.00 hour4.00 hourInjection
Moisture Content 0.20 %0.20 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Release agent
Agency RatingsISO, 1043 PA66
AppearanceNatural Color
FormsPellets
Processing MethodInjection Molding
RegionNorth America, Europe

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PASCE8517 / 296301

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.