MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Pressure Seal 19811 Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Compound 19811 is an 80 durometer salmon colored general purpose Silicone elastomer. It exhibits good resistance to heat and compression set, it has excellent low temperature flexibility. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 5 GE 809 A19 B37 EO16 EO36 F19 G11 EA14
AMS 3305E
ZZ-R-765 Class 2a & 2b Grade 80
A-A-59588 Class 2a & 2b Grade 80

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 82
 63
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
 79
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #1
 79
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 79
@Temperature 175 °C,
Time 252000 sec
ASTM Oil #1
 82
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 86
@Temperature 225 °C,
Time 79200 sec
Heat Aged
 87
@Temperature 225 °C,
Time 252000 sec
Heat Aged
Tensile Strength 1291 psi
 426 psi
@Temperature 175 °C,
Time 252000 sec
ASTM Oil #1
 1038 psi
@Temperature 225 °C,
Time 252000 sec
Heat Aged
 1061.2 psi
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
 1137.4 psi
@Temperature 225 °C,
Time 79200 sec
Heat Aged
 1155.4 psi
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
 1216.1 psi
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 1230.3 psi
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #1
Elongation, Ultimate 146 %
 113 %
@Temperature 225 °C,
Time 252000 sec
Heat Aged
 121 %
@Temperature 225 °C,
Time 79200 sec
Heat Aged
 125 %
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #3
 129.1 %
@Temperature 100 °C,
Time 252000 sec
ASTM Oil #1
 137.97 %
@Temperature 150 °C,
Time 252000 sec
ASTM Oil #1
 137.97 %
@Temperature 175 °C,
Time 252000 sec
ASTM Oil #1
 149.9 %
@Temperature 100 °C,
Time 252000 sec
Distilled water aged
100% Modulus 989 psi
Tear Strength 68.0 pliDie B
Compression Set 10.4 %
@Temperature 175 °C,
Time 79200 sec
Solid
 11.5 %
@Temperature 150 °C,
Time 252000 sec
Solid
 12.2 %
@Temperature 175 °C,
Time 79200 sec
Plied
 12.4 %
@Temperature 100 °C,
Time 79200 sec
Plied
 17.7 %
@Temperature 150 °C,
Time 252000 sec
Plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -104 °F
Shrinkage -3.10 %
@Temperature 225 °C,
Time 252000 sec
Volume, Heat Aged
 -2.30 %
@Temperature 225 °C,
Time 79200 sec
Volume, Heat Aged
 0.20 %
@Temperature 100 °C,
Time 252000 sec
Volume, Distilled water aged
 2.2 %
@Temperature 175 °C,
Time 252000 sec
Volume, ASTM Oil #1
 2.3 %
@Temperature 100 °C,
Time 252000 sec
Volume, ASTM Oil #1
 2.3 %
@Temperature 150 °C,
Time 252000 sec
Volume, ASTM Oil #1
 31.3 %
@Temperature 150 °C,
Time 252000 sec
Volume, ASTM Oil #3
 
Descriptive Properties
ColorSalmon

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL174 / 318384

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.