MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger Tecapeek® CMF white Polyetheretherketone, Ceramic Filled
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes:
  • high dimensional stability
  • good machinability
  • high strength
  • high stiffness
  • low thermal expansion
  • low burring
  • good heat deflection temperature
  • very good thermal stability
Target Industries:
  • electrical engineering
  • precision engineering
  • semiconductor technology
  • vacuum technology

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.63 g/cc0.0589 lb/in³
Moisture Absorption 0.0300 %
@Time 86400 sec
0.0300 %
@Time 24.0 hour
ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 102102ASTM D 785
Tensile Strength at Break 105 MPa15200 psi50 mm/min; DIN EN ISO 527-2
Tensile Strength, Yield 97.368 MPa14122 psiASTM D 638
Elongation at Break 4.85 %4.85 %ASTM D 638
Elongation at Yield 3.0 %3.0 %50 mm/min; DIN EN ISO 527-1
Modulus of Elasticity 8.46063 GPa1227.11 ksiASTM D 638
Flexural Strength 163.01 MPa23642 psiASTM D 790
Flexural Modulus 5.40263 GPa783.585 ksiASTM D 790
Compressive Yield Strength 142.80 MPa
@Strain 10 %
20712 psi
@Strain 10 %
ASTM D 695
Compressive Strength 12.79 MPa
@Strain 1 %
1855 psi
@Strain 1 %
ASTM D 695
Compressive Modulus 2.31229 GPa335.369 ksiASTM D 695
Izod Impact, Notched 0.352 J/cm0.660 ft-lb/inASTM D 256
Izod Impact, Unnotched 8.131 J/cm15.23 ft-lb/inASTM D 256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 3.50e+15 ohm-cm3.50e+15 ohm-cmASTM D 257
Surface Resistivity per Square 5.20e+15 ohm5.20e+15 ohmASTM D 257
Dielectric Constant 4.71
@Frequency 1e+6 Hz
4.71
@Frequency 1e+6 Hz
ASTM D 150
Dielectric Strength 6.61 kV/mm168 kV/inASTM D 149
Dissipation Factor 0.0032
@Frequency 1e+6 Hz
0.0032
@Frequency 1e+6 Hz
ASTM D 150
 
Thermal PropertiesMetricEnglishComments
CTE, linear  40.1 µm/m-°C
@Temperature 22.8 - 60.0 °C
22.3 µin/in-°F
@Temperature 73.0 - 140 °F
ASTM E 831
 40.9 µm/m-°C
@Temperature 22.8 - 100 °C
22.7 µin/in-°F
@Temperature 73.0 - 212 °F
ASTM E 831
 46.4 µm/m-°C
@Temperature 100 - 150 °C
25.8 µin/in-°F
@Temperature 212 - 302 °F
ASTM E 831
Thermal Conductivity 0.375 W/m-K2.60 BTU-in/hr-ft²-°FASTM E1530
Melting Point 339 °C643 °F
Maximum Service Temperature, Air 260 °C500 °FLong Term
 260 °C500 °FShort Term
Flammability, UL94 V-0V-0
 
Descriptive Properties
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8179 / 319107

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.