MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C18620, ANNEAL Temper, Pipe
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: ANNEAL

Fabrication Properties: Excellent Suitability – Soldering, Brazing, Capacity for Being Cold Worked, Capacity for Being Hot Formed

Typical Uses: Automotive & Aircraft-air, hydraulic, gas & oil lines; Air Conditioner Tube, Steam Lines; Heater Elements; Evaporator Tube, Plumbing Tube

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.321 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 85
@Load 0.500 kg
Tensile Strength >= 36.0 ksi
 43.0 ksiTypical
Tensile Strength, Yield >= 14.0 ksi0.2% Offset
 21.0 ksi0.2% Offset, Typical
Elongation at Break 40 %
Machinability 20 %
Forgeability 68 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000200 ohm-cm85% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µin/in-°F
@Temperature 20.0 - 300 °C
Thermal Conductivity 196 BTU-in/hr-ft²-°F
Melting Point 1967 - 1976 °F
Solidus 1967 °F
Liquidus 1976 °F
 
Component Elements PropertiesOriginal ValueComments
Cobalt, Co 0.14 - 0.21 %
Copper, Cu >= 99.4 %
Nickel, Ni 0.020 - 0.060 %
Phosphorus, P 0.040 - 0.075 %
Tin, Sn 0.030 - 0.15 %
Zinc, Zn 0.020 - 0.10 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC18620x1 / 291656

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.