Appearance: Gray Cure: Heat cure Product Benefits: - One component
- Non-conductive
- General purpose
- Sag resistant
- Low viscosity
- Non-abrasive
- Excellent dielectric properties
- Long shelf life at room temperature
- Excellent resistance to heat and water
- High adhesion strength at elevated temperatures
Application: Adhesive and Sealant Filler Type Silver Typical Assembly Applications: Insulation of copper and other materials and Attaching leads to coils Key Substrates: Copper, Rigid plastics and Other metals LOCTITE ABLESTIK G 500 is a general purpose epoxy adhesive and sealant that cures to a high gloss finish. Information provided by Loctite® |