MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
American Elements Rhenium Nanoparticles
Categories: Metal; Nonferrous Metal; Pure Element

Material Notes: General Description

Rhenium (Re) Nanoparticles, nanodots or nanopowder are brown spherical high surface area metal particles. Nanoscale Rhenium Particles are typically 20 - 100 nanometers (nm) with specific surface area (SSA) in the 1 – 3 m 2 /g range. Nano Rhenium Particles are also available in Ultra high purity and high purity and coated and dispersed forms. Applications for Rhenium nanocrystals include for immunotherapy of solid tumors, in a nucleation layer of palladium and rhenium nanoparticles in-between a nanostructure copper pad surface to create an electrical connection that has superior diffusion barrier and adhesion properties numerous uses in catalysts, in magnetically targeted therapy and as a Magnetic Nanopowder, in polymer membranes to create Active Polymer Membranes and in other coatings, plastics, nanofiber and textiles and in nanowire and other catalysis applications.

Key Words: Formula: Re; CAS Number: 7440-15-5
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 0.020 - 0.10 µm
Specific Surface Area 1.0 - 3.0 m²/g
Molecular Weight 186.21 g/mol
 
Descriptive Properties
AppearanceBrown

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

EJAMER69 / 5552

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.