MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Kraiburg TPE THERMOLAST® K TC5MGZ Black TPE  (Unverified Data**)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes:
  • Adhesion to technical thermoplastics
  • Adhesion to ABS, SAN, ASA, PC, PC/ABS, PC/PBT, PBT, PET, PETG, PMMA
  • For patent free comolded parts
  • Good flow characteristics
  • Excellent adhesion even with soft compounds
  • UL94 HB listed compounds available

Typical Applications:

  • Electric and electronic components
  • Seals
  • Coverings
  • Design and functional elements
  • Handles (for hand tools, power tools, etc.)
  • In the automotive industry (air inlet piping, cowl, stop button, door sill, etc.)

Material Advantages:

  • Excellent adhesion without pretreatment (depending on geometry and processing)
  • Adhesion to many engineering thermoplastics
  • Easy to color
  • Tactile surface (soft touch)
  • Excellent flow characteristics

Processing:

  • Processing on 2K injection molding machines (many grades also for insert molding)
  • Low back pressure
  • High shear force is beneficial for flow behavior
  • High injection speed and pressure

Information provided by Kraiburg TPE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccDIN 53479
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 53DIN 53505
Tensile Strength at Break 3.60 MPaDIN 53504
Elongation at Break 423 %DIN 53504
Tear Strength 19.2 kN/mDIN 53515
Compression Set 82 %
@Temperature 70.0 °C
24 hours; ISO 815
 86 %
@Temperature 100 °C
24 hours; ISO 815
 37 %
@Temperature 23.0 °C,
Time 259000 sec
ISO 815
 
Processing PropertiesOriginal ValueComments
Processing Temperature 180 - 240 °C
Mold Temperature 40.0 - 60.0 °C
Drying Temperature 60.0 - 80.0 °CPre-drying
Dry Time 2 - 4 hourPre-drying
 
Descriptive Properties
ColorBlack

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Eastman Llumar E1220 SR CDF (Silver) Window Film
Total PPC 4720 WZ Polypropylene, Impact Copolymer
Miracll E355D Thermoplastic Polyurethane (TPUR), Polyester Grade
Envalior Arnitel® EM460 TPC-ET, Injection Molding or Extrusion Grade

PKRAIB021 / 49168

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.