423 Graphite Powder is a fine black powder that can be mixed with WEST SYSTEM epoxy to produce a low-friction exterior coating with increased scuff resistance and durability. Epoxy/graphite is commonly used as a bearing surface, and as a coating on rudders and centerboards, or on the bottoms of racing craft that are dry sailed. It does not provide antifouling qualities. The epoxy/graphite mixture can also be used in teak deck construction to simulate the look of traditional seams and to protect the epoxy from sunlight. Cures to a black color. Add to mixed resin/hardener at the rate of up to 10% by volume (approximately 5.7 oz. per B group).Information provided by Gougeon Brothers, Inc. |