MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CHT QSil Beyond X1 Transparent Liquid Silicone Elastomer
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Description: The product is a transparent and colorless silicone formulation and is ideal for optical applications. The viscosity profile enables excellent flow around components and is excellent for potting complex parts. The chemical composition results in a cured product that is hydrolytically stable as well as reversion resistant. The silicone elastomer provides electrical insulation and physical shock resistance of components and enables environmental protection.

Key Features

  • Low linear shrinkage
  • Non-yellowing catalyst system
  • Self-bonding without primer, requires cure at elevated temperature to build adhesion and develop full physical properties
  • Meets Mil-I-81550C (type II) standard
Application: Solar panel encapsulating layer

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³B
 1.01 g/cc0.0365 lb/in³A
Brookfield Viscosity 650 cP650 cPB
 3400 cP3400 cPMixed
 4000 cP4000 cPA
Storage Temperature <= 38.0 °C<= 100 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545ASTM D2240-95
Tensile Strength 5.20 MPa754 psiISO 37
Elongation at Break 100 %100 %ISO 37
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.70e+10 ohm-cm1.70e+10 ohm-cmASTM D-257
Dielectric Constant 2.692.69ASTM D-150
Dielectric Strength 19.7 kV/mm500 kV/in
Dissipation Factor 0.000600.00060ASTM D-150
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 1.26 J/g-°C0.300 BTU/lb-°F
Thermal Conductivity 0.180 W/m-K1.25 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 204 °C399 °F
Minimum Service Temperature, Air -55.0 °C-67.0 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4061.406
 
Processing PropertiesMetricEnglishComments
Cure Time 60.0 min
@Temperature 150 °C
1.00 hour
@Temperature 302 °F
Gel Time >= 1440 min>= 1440 min
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
AppearanceAddition
ColorTransparent and colorlessA
 Transparent and colorlessB
 Transparent and colorlessCured Product
Mix Ratio10:1By Weight
RheologyLiquid, Newtonian

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHTSIL058 / 314541

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.