MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Versalis Pharmalene® MP 30 PH Low Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Molded

Material Notes: Pharmalene MP 30 PH is a medium fluidity low density polyethylene (LDPE) without additives, obtained by high pressure autoclave process. It is produced according to good manufacturing practices (GMP) and is mainly used for injection molding. Application: Pharmalene MP 30 PH is intended for the use within pharmaceutical sector and is characterized by a good balance between flow ability and rigidity. Pharmalene MP 30 PH is recommended for high gloss surface and medium thickness articles. Pharmalene MP 30 PH is suitable for the production of pharmaceutical master batches and caps & closures.

Information provided by Versalis.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ISO 1183
Melt Flow 7.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
7.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5050Injection Molded; ISO 868 A
Tensile Strength, Yield 12.0 MPa1740 psiISO 527
Flexural Modulus 0.200 GPa29.0 ksiISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 112 °C234 °FManufacturer method
Vicat Softening Point 92.0 °C
@Load 1.00 kg
198 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -65.0 °C<= -85.0 °FASTM D 746
 
Processing PropertiesMetricEnglishComments
Processing Temperature 160 - 200 °C320 - 392 °FBarrel; Injection Molding
Mold Temperature 10.0 - 30.0 °C50.0 - 86.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENF9863 / 265657

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.