MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ASI® 3 Adhesive Accelerator
Categories: Fluid; Other Engineering Material; Catalyst/Initiator

Material Notes: Quick Tac Accelerator have been developed as a treating agent for use with the ADVANCED PERFORMANCE family of instant adhesive products. If faster setting speeds are desired, QUICK TAC will aid the curing process and give exceptionally faster set times. When curing beads or in applications where the adhesive is not between two parts, it will allow for faster uniform curing. QUICK TAC will aid the bonding of porous materials such as fabrics or woods. It is useful when bonding acidic surfaces or in low humidity conditions promoting consistent curing times. Used for wire tacking , silk screening , or in loudspeaker assembly. Using QUICK TAC will enable the adhesive to fill gaps up to 0.20". QUICK TAC can be applied by brushing or spraying.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.790 g/cc
Viscosity 3.0 cP
 
Thermal PropertiesOriginal ValueComments
Boiling Point 180 - 181 °F
Flash Point 53.0 °F
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 MonthIn original sealed container when properly stored.
 
Descriptive Properties
Baseisopropyl alcohol
Color / appearanceclear/amber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9075 / 233442

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.