MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Vyncolit BXE650 Inorganic Filled Phenolic Molding Compound
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Phenolic; Phenolic, Novolac, Mineral Filled

Material Notes: Novolac resin based, inorganic filled. Excellent isotropic properties and superior dimensional stability. High mechanical properties even at elevated temperatures

Information provided by Sumitomo Bakelite North America, Inc.

Key Words: PF-(GB+GF)75
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.750 g/ccISO 60
Density 1.99 g/ccISO 1183
Water Absorption 0.050 %ISO 62
Linear Mold Shrinkage 0.0018 cm/cmISO 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 119 MPaISO 527-1
Elongation at Break 0.59 %ISO 527-1
Tensile Modulus 23.0 GPaISO 527-1
Flexural Strength 240 MPaISO 178
Flexural Modulus 21.0 GPaISO 178
Compressive Strength 434 MPaISO 604
Charpy Impact Unnotched 13.6 kJ/m²ISO 179-1
Charpy Impact, Notched 2.90 kJ/m²ISO 179-1
Coefficient of Friction, Dynamic 0.54
Coefficient of Friction, Static 0.56
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.10e+14 ohm-cmIEC 60093
Surface Resistance 2.50e+12 ohmIEC 60093
Dielectric Strength 20.0 kV/mmIEC 60243-1
Comparative Tracking Index 225 VIEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 16.0 µm/m-°CTMA
CTE, linear, Transverse to Flow 24.0 µm/m-°CTMA
Thermal Conductivity 0.510 W/m-KASTM E1461
Deflection Temperature at 1.8 MPa (264 psi) >= 250 °CISO 75 Af
Deflection Temperature at 8.0 MPa 178 °CISO 75 Cf
Flammability, UL94 V-0
@Thickness 3.00 mm
 V-0
@Thickness 1.50 mm
Shrinkage 0.040 %Post Shrinkage; ISO 2577
 
Descriptive Properties
ColorBlack
Molding MethodCompression
 Injection
 Transfer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PVYNC945 / 142720

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.