LFI 2119 is a low density polyethylene, with excellent optical properties. This grade offers a high output and excellent draw down and specially designed for general purpose thin films. Typical Applications: LFI 2119 is recommended for blown film extrusion. This product is suitable for manufacture of general purpose LDPE film packaging and general lamination films. Property data based on 25 µm blown film produced at a melt temperature of 170°C and 3 BUR using 100% LFI2119. Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co. |