MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer CXT17EX PC (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN™ CXT17EX resin is a High Heat Polycarbonate Copolymer Resin with Vicat of 170°C and crystal clear transparency. This resin is optimized for sheet and film extrusion applications, has a low plateout and a broad processing window with limited yellowing. It is available in limited transparent colors.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/ccASTM D792
Density 1.21 g/ccISO 1183
Moisture Absorption 0.300 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.30 %ISO 62
Linear Mold Shrinkage, Flow 0.0070 - 0.0095 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0070 - 0.0095 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 27 g/10 min
@Load 2.16 kg,
Temperature 330 °C
MVR [cc/10 min]; ISO 1133
 30 g/10 min
@Load 2.16 kg,
Temperature 330 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 60.0 MPa50 mm/min; ASTM D638
 60.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 75.0 MPa50 mm/min; ASTM D638
 75.0 MPa50 mm/min; ISO 527
Elongation at Break >= 40 %50 mm/min; ASTM D638
 >= 50 %50 mm/min; ISO 527
Elongation at Yield 6.5 %50 mm/min; ISO 527
 7.0 %50 mm/min; ASTM D638
Tensile Modulus 2450 MPa1 mm/min; ISO 527
 2500 MPa5 mm/min; ASTM D638
Flexural Yield Strength 110 MPa2 mm/min; ISO 178
 120 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2450 MPa1.3 mm/min, 50 mm span; ASTM D790
 2500 MPa2 mm/min; ISO 178
Izod Impact, Notched 80.0 J/mASTM D256
 75.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 8.00 kJ/m²80*10*3; ISO 180/1A
 7.00 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 10.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 7.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 167 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 167 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 154 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 154 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 174 °CRate B/120; ASTM D1525
 174 °CRate B/120; ISO 306
Glass Transition Temp, Tg 175 °Chalf width; SABIC method
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.602ISO 489
Abbe Number 30ISO 489
Transmission, Visible 87 %
@Thickness 3.00 mm
ASTM D1003
 88 %
@Thickness 2.00 mm
ASTM D1003
 89 %
@Thickness 1.00 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CHopper Temperature
 90.0 - 150 °CCalibrator Temperature
Zone 1 160 - 230 °CMultiwall Sheet Extrusion
Zone 2 250 - 290 °CMultiwall Sheet Extrusion
Zone 3 280 - 345 °CMultiwall Sheet Extrusion
Adapter Temperature 80.0 - 130 °CMultiwall Sheet Extrusion
Die Temperature 270 - 350 °C
Melt Temperature 270 - 350 °CMultiwall Sheet Extrusion
Drying Temperature 135 °CMultiwall Sheet Extrusion
Dry Time 4.00 - 6.00 hourMultiwall Sheet Extrusion

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH91473 / 252597

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.