MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Röhm ACRYLITE® Softlight zk6BR df23 Acrylic polymer
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, Extruded

Material Notes: ACRYLITE® Softlight zk6BR df23, based on ACRYLITE® Resist zk6BR, is an impact modified molding compound characterized by diffuse scattering of light.

Typical properties of impact modified ACRYLITE® molding compound are

  • high break resistance and impact strength
  • improved resistance to stress cracking
  • good weather resistance
  • high surface hardness and mar resistance
  • the pleasant feel and sound of the moldings.
ACRYLITE® Softlight zk6BR df23 is characterized by the following special properties:
  • excellent light diffusion combined with excellent light transmittance
  • matte surfaces can be obtained by varying the extrusion parameters.
Application: Used for extruding profiles and sheets, but also for injection molding items for lighting engineering applications

Information provided by Roehm America LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccISO 1183
Melt Flow 1.3 g/10 min
@Load 3.80 kg,
Temperature 230 °C
1.3 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 46.0 MPa6670 psi50 mm/min; ISO 527
Elongation at Break 36 %36 %Nominal; ISO 527
Elongation at Yield 5.0 %5.0 %50 mm/min; ISO 527
Tensile Modulus 1.90 GPa276 ksi1 mm/min; ISO 527
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179/1
 
Thermal PropertiesMetricEnglishComments
CTE, linear 90.0 µm/m-°C50.0 µin/in-°FISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C210 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C199 °FISO 75
Vicat Softening Point 99.0 °C210 °FB / 50; ISO 306
Glass Transition Temp, Tg 109 °C228 °FISO 11357
Glow Wire Ignition Temperature 700 °C1290 °FIEC 60695-2
 
Optical PropertiesMetricEnglishComments
Transmission, Visible >= 81 %>= 81 %ISO 13468-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 230 - 260 °C446 - 500 °F
Mold Temperature 60.0 °C140 °FExtrusion
Drying Temperature <= 85.0 °C<= 185 °FPredrying
Dry Time 2.00 - 3.00 hour2.00 - 3.00 hourPredrying, Desiccant-Type Drier
 
Descriptive Properties
Half-Value Angle21DIN 5036

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PROHM9337 / 319954

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.