MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metal adhesives

(Viewing data as-entered. Click here to return)
Master Bond EP4G-80 One component, graphite filled epoxy
Categories: Polymer; Thermoset; Epoxy

Material Notes: Key Features:
  • Good electrical conductivity
  • Flowable
  • Convenient packaging
  • Meets NASA low outgassing certification
Product Description: Master Bond EP4G-80 is a one component, low viscosity, graphite filled epoxy that meets NASA low outgassing requirements. This material has exceptional flow properties and can be used for bonding, sealing and coating applications. Upon curing, it combines good thermal and electrical conductivity. EP4G-80 can be packaged in syringes or jars. Syringes are shipped in dry ice, stored in a cryogenic freezer, and are specified for one time use. Upon thawing, the epoxy should be used within 6-8 hours, and any remaining material discarded. When packaged in jars, there are no shipping restrictions, although it is recommended that the jars be stored in a refrigerator. For best results, after removing from the refrigerator, jars should be used within a 12 hour time frame. The jar can then be returned to the refrigerator to be used in the same manner. Regardless of the packaging, the epoxy cures readily in 60-90 minutes at 80°C. Post curing at 80°C for 1-2 hours will optimize properties. EP4G-80 bonds well to a wide variety of substrates such as metals, composites, ceramics and many plastics. The epoxy combines good dimensional stability, superb compressive strength, along with a high modulus. The volume resistivity ranges from 50 to 100 ohm-cm. It is very flowable, and can be used for specialty applications where graphite type electrical conductivity is needed. Graphite is a desirable filler material because it is non-metallic, provides reliable performance, and is also cost effective, especially when compared to silver. It resists water, oils, fuels, along with mild acids and bases. Its color is black. The service temperature range is -50°C to +175°C. EP4G-80 is an attractive option for a variety of applications including specialty OEM, aerospace, opto-electronics, among others, where graphite conductivity and low outgassing are desirable.

Product Advantages:

  • One component
  • Will not cure until heated
  • Curing temperature 80°C
  • Low viscosity
  • Graphite conductivity
  • Passes NASA low outgassing
Best usage for syringes: within 6-8 hours after removing from freezer; discard leftover material

Best usage for jars: within 12 hours after removing from refrigerator, gently stir; return to refrigerator to be used again

Information provided by Master Bond.

Vendors: Master Bond is a leading manufacturer of adhesives, sealants, coatings and potting compounds. Master Bond’s vast product line consists of over 3,000 epoxy, polyurethane, silicone, cyanoacrylate and latex adhesives that vary in viscosity, cure speed, strength, chemical resistance, electrical properties, etc. Our custom adhesives offer design flexibility and provide excellent bonding performance. Visit www.masterbond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.30 g/cc
Viscosity 4000 - 10000 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75 - 85
Tensile Strength 2000 - 3000 psi
Elongation at Break <= 1.0 %
Tensile Modulus >= 750000 psi
Compressive Strength 22000 - 24000 psi
Adhesive Bond Strength 800 - 1000 psiTensile lap shear, Al to Al
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 50 - 100 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 10.0 - 12.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 175 °C
Minimum Service Temperature, Air -50.0 °C
Glass Transition Temp, Tg 130 - 140 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 - 90.0 min
@Temperature 80.0 °C
Optimal, followed by 1-2 hours at 80°C
Shelf Life 3.00 - 6.00 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMASTM5903 / 306792

Metal adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.