MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Momentive Performance Materials Silopren LSR 2841 TP 3601 Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Silopren LSR 2841 TP 3601 is a two-component liquid silicone rubber for the production of key pads by injection molding processes. Due to the low hysteresis of Silopren LSR 2841 TP 3601 the key pads shows especially long service life.

Features: high reactivity. Long service life at dynamic stress. Very good flow ability. Excellent dielectric behavior over a wide range of temperatures. High stability and flexibility at low temperatures. Excellent stability to ozone and ultraviolet light. Not readily combustible, does not melt or drip. Easy to add pigment with LSR Color Pastes.

Applications: Because of the outstanding properties Silopren LSR 2841 TP 3601 liquid silicone rubber is particularly suitable for the production of key pads and articles with high dynamic stress like diaphragms

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccDIN 53 479 A
Viscosity 120000 cPUncured. A- part; DIN 53018
 120000 cPUncured. B-part.; DIN 53018
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 40DIN 53 505
Tensile Strength 6.00 MPaDIN 53 504 S2
Elongation at Break 550 %DIN 53 504 S2
Tear Strength 21.4 kg(f)/cmASTM D 624
 
Electrical PropertiesOriginal ValueComments
Arc Resistance <= 250 secDIN VDE 0441, part 1
 
Processing PropertiesOriginal ValueComments
Processing Temperature 175 °C
@Time 601 sec
Vulcanization as Tested; Die B
Pot Life 4320 min
@Temperature 20.0 °C
Closed vessel
 
Descriptive Properties
ColorColorlessUncured. A-part.
 ColorlessUncured. B-part
Mix Ratio1:1 A:BAs Tested
Tracking Resistance1A 3.5 Class

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9982 / 265797

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.