MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Go Yen Chemical GYC TOTM
Categories: Other Engineering Material

Material Notes: GYC TOTM has low volatility and low migration and its electric resistivity and heat resistance are excellent.

Introduction: TOTM is produced by esterifying 2-Ethylhexanol and TrimelliticAnhydride. TOTM has low volatility and low migration and its electric resistivity and heat resistance are excellent. The wire and cable to which TOTM is applied in the process can pass USA s UL 62105°C class. TOTM’s migration and water extraction are lower than those of DIDP. To compare with DOP at the same flexibility, TOTM’s cold resistance is lower. With respect to PVC plastisol, under the condition of same flexibility, the viscosity of plastisol made with TOTM base is lower to that made with DIDP. As regards stability, since TOTM plastisol changes less than DOP, it is considered more stable than DOP.

Usage:

  • Wires & Cables
  • Leather & Clothes
  • Gloves
  • Shoes
  • Construction materials
  • PVC Plastisols

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.987 - 0.999 g/cc(20/20)
Viscosity 244 cP
@Temperature 30.0 °C
Molecular Weight 547 g/mol
 
Chemical PropertiesOriginal ValueComments
Acid Value <= 0.20[mgKOH/g]
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+11 ohm-cm
@Temperature 30.0 °C
 
Thermal PropertiesOriginal ValueComments
Boiling Point 430 °C
@Pressure 0.101 MPa
Flash Point 426 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.478 - 1.488
 
Descriptive Properties
Color<100APHA
Freezing point-55°C
Heat loss<0.15125°Cx3hr
Properties303-313 mgkOH/gEsterification number

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGOYEN904 / 267212

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.