MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC CYCOLAC DL100 ABS (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; ABS Polymer

Material Notes: CYCOLAC DL100 is a high heat, high impact, low emissions ABS/PC blend.

Information provided by SABIC Innovative Plastics for the Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmon Tensile Bar; SABIC Method
Melt Flow 7.0 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ISO 1133
 8.0 g/10 min
@Load 5.00 kg,
Temperature 260 °C
cm^3/10 min Melt Volume Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 104ASTM D 785
Hardness, H358/30 91.0 MPaISO 2039-1
Tensile Strength, Yield 44.0 MPaType I, 5 mm/min; ASTM D 638
 45.0 MPa50 mm/min; ISO 527
 46.0 MPa5 mm/min; ISO 527
Elongation at Break 10 %50 mm/min; ISO 527
 60 %5 mm/min; ISO 527
 90 %Type I, 5 mm/min; ASTM D 638
Elongation at Yield 3.4 %50 mm/min; ISO 527
 3.5 %5 mm/min; ISO 527
Tensile Modulus 2200 MPa1 mm/min; ISO 527
 2240 MPa5 mm/min; ASTM D 638
Flexural Yield Strength 69.0 MPa2 mm/min; ISO 178
Flexural Modulus 2250 MPa2 mm/min; ISO 178
Izod Impact, Notched 700 J/m
@Temperature 23.0 °C
ASTM D 256
 550 J/m
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D 256
Izod Impact, Notched (ISO) 15.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 35.0 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 14.0 kJ/m²
@Temperature -30.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
 34.0 kJ/m²
@Temperature 23.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 98.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 98.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 104 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 105 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 87.0 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 88.0 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
 90.0 °C
@Thickness 6.40 mm
unannealed; ASTM D 648
Vicat Softening Point 105 °CRate B/50; ISO 306
 107 °CRate B/120; ISO 306
UL RTI, Electrical 60.0 °CUL 746B
UL RTI, Mechanical with Impact 60.0 °CUL 746B
UL RTI, Mechanical without Impact 60.0 °CUL 746B
Flammability, UL94 HB
@Thickness 3.00 mm
2nd value; UL 94
 HB
@Thickness 1.50 mm
UL 94

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Desmopan® 6080A TPU
Huntsman IROGRAN® A 70 E 4675 Polyester-Based TPU-High Performance Grade
Envalior Durethan® BKV 115 H3.0 DUS008 000000 Nylon 6 (PA6), 15% Glass Fiber Reinforced, Dry
Envalior Durethan® BC 40 SR2 000000 Nylon 6 (PA6), Dry
Envalior Durethan® BC 40 SR2 000000 Nylon 6 (PA6), Conditioned

PSABI46003 / 187088

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.